Line 15: | Line 15: | ||
==== Toner Transfer ==== | ==== Toner Transfer ==== | ||
- | __Works.__ | + | __Works.__ |
The traces are laser-printed in reverse onto some sort of glossy paper (e.g. magazine or photo paper), then transferred to a copper-clad board using a hot clothing iron or t-shirt press. The traces transfer to the board and act as an etch-resist. | The traces are laser-printed in reverse onto some sort of glossy paper (e.g. magazine or photo paper), then transferred to a copper-clad board using a hot clothing iron or t-shirt press. The traces transfer to the board and act as an etch-resist. | ||
+ | [[http:// | ||
Issues: | Issues: | ||
Line 170: | Line 171: | ||
==== 3D Printer ==== | ==== 3D Printer ==== | ||
- | __Has potential.__ | + | __Doesn' |
- | Single layer of plastic laid down as etch resist. | + | Single layer of plastic laid down as etch resist. Laying down conductive material may soon be an option. |
Issues: | Issues: | ||
* Accuracy. Print heads tend to be at least 0.35mm. | * Accuracy. Print heads tend to be at least 0.35mm. | ||
+ | * Plastic shrinkage. | ||
+ | * Will not stick to copper. | ||
===== Mechanical ===== | ===== Mechanical ===== |